ER309MoL for Duplex-SS316 joint
ER309MoL for Duplex-SS316 joint
(OP)
Can we use ER309MoL filler wire for welding SS316 and Duplex steel?
INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS Come Join Us!Are you an
Engineering professional? Join Eng-Tips Forums!
*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail. Posting GuidelinesJobs |
ER309MoL for Duplex-SS316 joint
|
RE: ER309MoL for Duplex-SS316 joint
RE: ER309MoL for Duplex-SS316 joint
The corrosion resistance of the weld will be less than for either of the base materials.
= = = = = = = = = = = = = = = = = = = =
Corrosion never sleeps, but it can be managed.