INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Hastolloy-C22 flange

Hastolloy-C22 flange

Hastolloy-C22 flange

(OP)
Dear friends,

Which flange group in ASME B16.5 can cover the B564-N06022(Hastelloy-C22) flange?
There is no B564-N06022 material in Table 1A of ASME B16.5.

RE: Hastolloy-C22 flange

onrush,

In my ASME B16.5-2003, the material you are looking for is listed with Material Group 3.8 of Table 1A on page 5, but is apparantly covered by ASTM B462 instead of ASTM B564. Review those ASTM standards for their scope of materials.

Regards,

NozzleTwister
Houston, Texas

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources