INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Dimensional Tolerance on 6061 T6511

Dimensional Tolerance on 6061 T6511

Dimensional Tolerance on 6061 T6511

(OP)
Can anyone give me the dimensional tolerance on a Alumiunum 6061 T6511 Flat bar 2" Wide X 5/16" Thick?  I have a set of ASTM standards and am using ASTM B221 to spec the material.  ASTM B221 refers to ANSI H35.2 for size tolerances.  I do not have the ANSI standard for this.  Can anyone help me out?  Thanks.

Pete Yodis

RE: Dimensional Tolerance on 6061 T6511

(OP)
Goahead,

     Thanks for the reply.  Do you know if the tolerances listed on that site are characteristic of ANSI H35.2 as referenced from ASTM B221?  I did not find any mention on the site of adherence to any particular specification regarding tolerances, just a general statement; "tolerances are based on published standards used throughout the industry."

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources