fire resistance interior panels
fire resistance interior panels
(OP)
Does anyone knows if the interior aircraft panel (i.e.partitions, galleys, etc) have any damage resistance requirements or is the material used simply selected (beside its mass of course) on the basis of its fire resistance and heat release?





RE: fire resistance interior panels
Nigel Waterhouse B Eng (Hon's)
Can-Am Aerospace,LLC, Canadian Aircraft Certification Centre
www.canamaero.com
RE: fire resistance interior panels
This sound quite subjective, do you know if there are any test methods or standards to define their resistance? (i.e. the break strength or maximum curving)
RE: fire resistance interior panels
Nigel Waterhouse B Eng (Hon's)
Can-Am Aerospace,LLC, Canadian Aircraft Certification Centre
www.canamaero.com
RE: fire resistance interior panels
RE: fire resistance interior panels
Debodine's comments need to be considered also.
Nigel Waterhouse B Eng (Hon's)
Can-Am Aerospace,LLC, Canadian Aircraft Certification Centre
www.canamaero.com
RE: fire resistance interior panels
This, after some very premature test failures in galleys designed for a start-up airline.
There was some excellent guidance given out at the Atlanta DER conference a few years ago on interior monument substantiation. That presentation has since been made available from many ACOs on CD.
Ask for it; it will help you get through the certification process much more smoothly.