INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Simulation of the Tension Strength Test Composites matierial

Simulation of the Tension Strength Test Composites matierial

Simulation of the Tension Strength Test Composites matierial

(OP)
madmonkey (Automotive)      
16 May 05 14:15
HI ALL
i am trying to simulate in ANSYS the Tension Strength Test (TST).The TST has been already done. i got the values(grapf stress-strain).
Now im traing to create the simulation of the TST in ANSYS. I got all the materials values:

fiber E=73GPa, V(volume)fiber=0.32% Poisson=0.25
matrix  e=3Gpa Poisson=0.316

number of layers 14 (in ansys i use 29 layers, first and last layers are half height of matrix, plus another 13 of matrix in full heihgt and 14 layers of fibers)
example
1st layer half height of matrix
2nd layer fiber full height
3rd layer matrix full height
...
29th layer half height of matrix


i got the dimension of the sample (whole and the middle section).I'm modeling only the middle section.
i'm using the element SOLID46.
but the solution is different as a TST.

test value  for the composite is around 16GPa
but in Ansys it is only 3GPa (look like the same as a E of matrix)

any tips where i make the mistake?

thanks for all answers

Vladimir Zachar

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources