INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Meaning of "UIN" as applied to surface prep

Meaning of "UIN" as applied to surface prep

Meaning of "UIN" as applied to surface prep

(OP)
Can anyone tell me what "UIN" means as applied to surface
prep for moment connections?

RE: Meaning of "UIN" as applied to surface prep

"The roughness of a surface is measured in micro inches (uin), or micrometers (um).  One micro inch is equal to one one-millionth of an inch, as one micrometer equals one one-millionth of a meter.  The translation from standard to metric is: one micro inch =.025 micrometer; from metric to standard, one micrometer= 40 micro inches.  Within this scale every surface has roughness."

A google search provided this result. hope it helps.

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources