Wich kind of heat treatment is good for kon krusher
Wich kind of heat treatment is good for kon krusher
(OP)
Wich kind of heat treatment is good for kon krusher with C-0,45%,Mn-11%,Si-1%,Cr-1,3%,Mo-0,6%,Ni-1,5%.Work time is 200 Hours.
INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS Come Join Us!Are you an
Engineering professional? Join Eng-Tips Forums!
*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail. Posting GuidelinesJobs |
Wich kind of heat treatment is good for kon krusher
|
RE: Wich kind of heat treatment is good for kon krusher
RE: Wich kind of heat treatment is good for kon krusher
have you any information about heat treatment temperature and time of API5L Gr.X60 steel?
My question is about recovery,recristalisation & growth temperature and holding time.(for achieving to fine grain structure of welded groove joint by E8018 electrode in welding area which As per my syudies ,base structure of fusion zone,HAZ and base metal is ferritic and in part of FZ & HAZ areaes Bainitic structure(Witdmanstatan) has been observed.
Please be informed about chemical composition of above mentiond Carbon-Manganese Steel:
%C:Max. 0.26
%Mn:Max. 1.25
%S,P<0.030
Thanks for your help,
Regards
Kayvan
RE: Wich kind of heat treatment is good for kon krusher
RE: Wich kind of heat treatment is good for kon krusher
RE: Wich kind of heat treatment is good for kon krusher
RE: Wich kind of heat treatment is good for kon krusher