Material Standard - NORSOK Standard "Y03"
Material Standard - NORSOK Standard "Y03"
(OP)
We are taking delivery of a number of high pressure caps with a material NORSOK Y03.
Anyone have any idea what this material relates to in real money?
Anyone have any idea what this material relates to in real money?





RE: Material Standard - NORSOK Standard "Y03"
The following link should give you more info.
http:/
pipingdesigner
www.pipingdesigners.com
RE: Material Standard - NORSOK Standard "Y03"
http://
Assume it is one of the 355 grades from EN 10025.
Steve Jones
Materials & Corrosion Engineer
http://www.pdo.co.om/pdo/
RE: Material Standard - NORSOK Standard "Y03"
I have found a Rev 2 of M-120 which states Y03 having:
NORSOK Grade = S355J2G3 / EN 10025 for plate & sections
&
NORSOK Grade = S355N1 / prEN 10225 for Tubulars
Why it is missing from M-120 Rev 4 is one of lifes little mysteries.