fuel gas pipes flushing
fuel gas pipes flushing
(OP)
We have troubles with our furnaces fuel gas system, frequent clogging problems in burners and their feeding piping branches..so we are considering a flushing of the pipes
we used to do it with steam (3-4 bar), but got no results.
is there any means to use a more efficient solution to flush these pipes?
we used to do it with steam (3-4 bar), but got no results.
is there any means to use a more efficient solution to flush these pipes?





RE: fuel gas pipes flushing
RE: fuel gas pipes flushing
I did some analysis on deposits sample:
Iron: 24.4%
Manganese: 0.14%
lead: 0.15%
zn: .04%
antimony: 0.07%
Cu: 0.02%
loss at 550°c: 22%