INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

PT timber???

PT timber???

PT timber???

(OP)
Has anybody ever come across a post-tensioned timber beam circa 1920? I'm investigating an old church that experiences excessive deflections in the sanctuary floor. The girders consist of a 2-ply 2x something, with a 1/2" space on each side, then another 2x something on each side - so a 4-ply beam with (2) 1/2" gaps. In each gap are what the owner referred to as conduits - I assumed for wiring or something. A contractor friend of mine who looked at it thought they might be tension rods....

Anyway, I was about to recommend that they either replace the existing beams or add columns in the basement to reduce deflections, but after hearing this about the tension rods, thought it might be possible to re-tension the rods of they have slipped over the past 85 years...

Any ideas would be greatly appreciated.

-Steve

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources