INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Costs of SS vs Hastelloy, etc

Costs of SS vs Hastelloy, etc

Costs of SS vs Hastelloy, etc

(OP)
Hi. I'm just looking for some ballpark figures for the relative cost of 304SS, 316SS, and Hastelloy for manufacturing chemical processing equipment and vessels etc. Just rough numbers...TIA!

Fran McConville

RE: Costs of SS vs Hastelloy, etc

Fran,

It's a little awkward to give the info you seek right now as it appears to be a seller's market coupled with the price of nickel doing silly things.  I have just heard that supplier quotations are being given with only a 15 day validity so it looks a little volatile at the moment.  Another result of oil at USD 50 per barrel?

Steve Jones
Materials & Corrosion Engineer
http://www.pdo.co.om/pdo/

RE: Costs of SS vs Hastelloy, etc

(OP)
Well, ok, Steve. I just mean, does Hastelloy generally cost twice as much as stainless, 10 times as much, 30 times as much....?

Fran McConville

RE: Costs of SS vs Hastelloy, etc

From costs obtained last week, the commonly used nickel base alloys range from about 2.5 to 4 times that of 304 SS.   

RE: Costs of SS vs Hastelloy, etc

Thanks Stan.  I have to ask Fran, why the jump from 304/316 straight up to Hastelloy?  That's two ends of the corrosion resistant alloy spectrum. Are they for the same environment?

Steve Jones
Materials & Corrosion Engineer
http://www.pdo.co.om/pdo/

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources