ASTM Piping materials in Hydrogen Cyanide environment
ASTM Piping materials in Hydrogen Cyanide environment
(OP)
We have to select piping and valve materials suitable for a hydrogen gas stream containing 95 mol% H2, 2%N2, 3%CH4, 0.25%H2O, 0.1%CH3CN, 0.01%HCN, 50ppm NH3. Design conditions are 33 barg at 100°C. We design units for hydrogen gas streams on a regular basis using carbon steel piping and valves. However the presence of the HCN combined with the water concerns us and raises the question should we be using stainless steel ? Does anyone have any input please ?





RE: ASTM Piping materials in Hydrogen Cyanide environment
I would probably specify 316 ss.