INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

looking for specific grade of aluminum, anticorodal-100

looking for specific grade of aluminum, anticorodal-100

looking for specific grade of aluminum, anticorodal-100

(OP)
i am working for a european scientist who requires
a grade of aluminum only found in europe. the material
is anticorodal-100. the composition, i think, is AlMgSil.
do you have a material with these specifications? i need
two rounds, 6" dia. x 1" thick.
i've been informed that this material is called 6063 here
in the u.s. and it is an extruded material only. so now
i'm looking for tube shapes, 6" o.d. x 1" wall, and
4.5" o.d. x 1" wall

kenn fasanella
kenn@research.nj.nec.com

RE: looking for specific grade of aluminum, anticorodal-100

Kenn,
Anticorodal-100 is a commercial ref for Allussuisse for the AlMgSi1 aluminum.
So, I thing you can get some more info in their web site or e-mailing them.

Andrade
jaandrade@isq.pt
Instituto de Soldadura e Qualidade

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources