Cracks are developed in concrete basement walls constructed @ six months ago. The length of wall is @ 47ft. There are several cracks developed on interior side from top to bottom. Also, there are cracks developed on exterior side from top to midheight of basement walls.
1.What may be the reasons for these cracks?Is it due to temperature changes, or is there any limitations on length of basement wall beyond which we have to provide expansion or control joints?
2. What are the reinforcement requirements to resist thermal stresses?
1.What may be the reasons for these cracks?Is it due to temperature changes, or is there any limitations on length of basement wall beyond which we have to provide expansion or control joints?
2. What are the reinforcement requirements to resist thermal stresses?






RE: Reasons for Cracks in Concrete Basement Walls
Knowing the expansion length, u can find out the strain produced and thereby the thermal stress by multiplying the strain by modulus of elasticity of concrete.
The reinforcement required can then be easily found out for this stress.
Minimum temperature reinforcement depends upon the thickness of wall. Reynolds Handbook can give the details.