I will repair oil storage tank ( roof only ) with special coating or painting because the roof has been corrosion.
We plan to repair with condition tank online ( no hot work permit )and temp. of oil is 140F. ( API 650 Tank )
Anybody know how to repair and what product will be used for this work.
if anybody have an information pls let me know.
We plan to repair with condition tank online ( no hot work permit )and temp. of oil is 140F. ( API 650 Tank )
Anybody know how to repair and what product will be used for this work.
if anybody have an information pls let me know.





RE: Roof tank repair
Is this carbon steel tank?
If you have internal corrosion problem, you should consider about the method of surface preparation. All corrosion scale and rust should be removed before apply the paint.
RE: Roof tank repair
Come back with physical dimensions of the tank.