Plastic wear
Plastic wear
(OP)
Does anybody know if PA66 GF35 is compatible with PPA GF30 PTFE15 regarding wear?
Enviromental conditions are T= -30 to 130 Celsius degrees and a normal force of about 4 N.
I don't know the speed of contact point, but I presume it's quite high.
Sure not constant, parts are subjected to a on/off cycle.
Parts are 2.5 mm thick.
Enviromental conditions are T= -30 to 130 Celsius degrees and a normal force of about 4 N.
I don't know the speed of contact point, but I presume it's quite high.
Sure not constant, parts are subjected to a on/off cycle.
Parts are 2.5 mm thick.






RE: Plastic wear
RE: Plastic wear
RE: Plastic wear
Regards
eng-tips, by professional engineers for professional engineers
Please see FAQ731-376 for tips on how to make the best use of Eng-Tips Fora.
RE: Plastic wear