'Carbon Graphite' Processing..?
'Carbon Graphite' Processing..?
(OP)
I've been lookin around to find the differences in Graphite and 'Carbon Graphite'.. the way carbon graphite is processed and its properties; but cud find none... can anybody pls help me in this!!!





RE: 'Carbon Graphite' Processing..?
RE: 'Carbon Graphite' Processing..?
Thanks for your reply rnd2.. hope to see more from all you guys.
RE: 'Carbon Graphite' Processing..?
There is amorphous carbon and graphite. Both are allotropes of carbon and have very different physical properties but the same chemical properties.
When "combined" they form a bonded composite material, not a new chemical compound.