INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Standards for Swedish steels??

Standards for Swedish steels??

Standards for Swedish steels??

(OP)
hello friends,

I have a problem regarding Swedish steels.

If we consider steel 1232 according to:  Metalinfo, ASM and some Swedish books, standard for 1232 is SIS 141232,

1- However I found in some places this specification
SS 141232 , do you knowo which one is valid SS or SIS?

2- I would also like to ask you about steel 1232-00, is it the same as 1232 or not. I found for example 1232-03 or 1232-04, but I have never seen 1232-00, I used always 1232, but today I found this name 1232-00. Is it the same (1232 and 1232-00)? the similar case is for 1311 and
1311-00

If you have any answer or hint where I should look for, I would really appreciate that.

thak you very much

RE: Standards for Swedish steels??

SIS, Swedish Standards Institute is the name of the standards developing organization based in Stockholm.  The official name of the standard is SIS SS 141232 Allmänt konstruktions- och tryckkärlsstål - SS-stål 12 32 or Structural and pressure vessel steel using the international title.  The -00, -04, etc. refer to individual grades within the standard.  You can obtain more information by visiting their website:

http://www.sis.se/DesktopFront.aspx

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.