INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

ASTM A106 GrB. What is the Temp and Press range

ASTM A106 GrB. What is the Temp and Press range

ASTM A106 GrB. What is the Temp and Press range

(OP)
Working for a tight company who wdon't like buying standards.

Can anyone let me know where I can get the Temperature and Pressure specification of ASTM A106 GrB pipe.

I am especially interested in the low temperature limits.

Regards,

Biggy

RE: ASTM A106 GrB. What is the Temp and Press range

Low temp is -20 F unless you do charpy testing and then only down to -50 F.

If you work for a company too tight to buy a $33 standard then I doubt they would pay for the charpy testing.

Check B31.3 or B31.8 for the change in allowable stresses for higher temps.

RE: ASTM A106 GrB. What is the Temp and Press range

team members

The Pressure and Temperature is listed on the approved Pining Classification Specification and all calculation support the Pressure and Temperature and components for the above material.

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources