Hrxn table for EMA and MMA
Hrxn table for EMA and MMA
(OP)
I'm having a problem trying to locate a solid reference for the heat of reaction for ethyl methacrylate and methyl methacrylate.
I am trying to calculate my heat of reaction for polymerization of EMA and MMA in my reactor vessels as part of my Risk Managment Plan determination.
I have found two Hrxn #'s for MMA of 13.5 Kcal/gm-mole, and 13.9 Kcal/gm-mole.
I haven't found anyhting for EMA yet. However, I know it's going to be around the same number. EMA will run slightly cooler than MMA.
Thank you for any help you can give me.
- Brian
I am trying to calculate my heat of reaction for polymerization of EMA and MMA in my reactor vessels as part of my Risk Managment Plan determination.
I have found two Hrxn #'s for MMA of 13.5 Kcal/gm-mole, and 13.9 Kcal/gm-mole.
I haven't found anyhting for EMA yet. However, I know it's going to be around the same number. EMA will run slightly cooler than MMA.
Thank you for any help you can give me.
- Brian
Why do today what you can put off till tomorrow?
Unless, today is your yesterday's tomorrow.