INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

BUNA-N (Nitrile) vs Natural rubber

BUNA-N (Nitrile) vs Natural rubber

BUNA-N (Nitrile) vs Natural rubber

(OP)
I'd like to get the pro and cons about BUNA-N (Nitrile) and Natural rubber for use as a gasket material on water and air.

Albion is recommanding natural black rubber for water (hot & cold) and also for air.
Albion also do ot recommand Nitrile for sunlight,ozone and weather...

My applications are inside of buildings with water or air.
And the purpose of my request is to eliminate our inventory of black natural rubber to avoid misuses of it as a gasket on systems with petroleum products.

I know that it can create problems if nitrile is used outside but it is not a concern for us.

Thanks

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources