A320 Strength
A320 Strength
(OP)
Have a stud made with ASTM A320-L7. What is the ultimate strength of this material?
INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS Come Join Us!Are you an
Engineering professional? Join Eng-Tips Forums!
*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail. Posting GuidelinesJobs |
|
RE: A320 Strength
UTS - 125 Ksi min