INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

ASTMA 487 GR 4QM and T24S

ASTMA 487 GR 4QM and T24S

ASTMA 487 GR 4QM and T24S

(OP)
Are the above grades of stainless steel suitable for use in an H2S environment.

Thanking you in anticipation.

RE: ASTMA 487 GR 4QM and T24S

ASTM A-487 grade 4QM and A-487 grade T24S do not exist. Grade 4Q (old designation) is not a stainless steel. It is a nickel-chrome-moly low alloy steel with less than 1% Nickel.

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources