INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Name that alloy

Name that alloy

Name that alloy

(OP)
Hello.

I have a custom made crucible steel that reads out something like this;
C .50-.55 Cr .7-.95 Mn .65-.9 Mo .45-.55 Ni 4.0-5.0 P .1 S .04 Si 1.8-2.0 V .05 Fe Balance.

What commercially available alloy, does this come closest to? Thanks, Gerald

RE: Name that alloy

It looks like a NiCrMoV tool steel.  Maybe a mold steel?  The one that I think of has Al instead of Si, it is age hardenable.
There are a bunch of similar European chemistries, but I don't know anything about those alloys.

= = = = = = = = = = = = = = = = = = = =
Corrosion never sleeps, but it can be managed.
http://www.trenttube.com/Trent/tech_form.htm

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources