INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Piercing and Blanking Aluminum Sheet

Piercing and Blanking Aluminum Sheet

Piercing and Blanking Aluminum Sheet

(OP)
I have a part currently being waterjet cut from sheet stock 3/16" thick.  Can anyone enlighten me to the problems we would experience in stamping these parts in a  die?  we have the press, the technology, and the orders for increasing capacity by stamping versus cutting.

RE: Piercing and Blanking Aluminum Sheet

cobra427,
what material, size, tolerance and quantity required you're looking at?

Best regards,
ct

RE: Piercing and Blanking Aluminum Sheet

Cobra 427,

my company makes tool steel and one of the biggest problems our customers have with aluminium is cold welding.

We use coatings for this nowadays.

Regards
Richard

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources