Rubber Lining Standard
Rubber Lining Standard
(OP)
Does any one know what happened to the ASTM Standard
D3486 - Standard Practice for Installation of Vulcanizable Rubber Tank Linings and Pipe Linings ?
I've got an old specification referencing this standard but cannot find it on the latest ASTM list. Is there a replacement for this standard ?
D3486 - Standard Practice for Installation of Vulcanizable Rubber Tank Linings and Pipe Linings ?
I've got an old specification referencing this standard but cannot find it on the latest ASTM list. Is there a replacement for this standard ?





RE: Rubber Lining Standard
I cannot help with ASTM Standard but if you do not find it you can possibly make use of British Standard 6374 whic seems to be our equivalent. Cheers DW