150 ksi threadbars in shear
150 ksi threadbars in shear
(OP)
Does anyone have experience using Dwyidag rod (ASTM A722 Fu=150ksi) as a shear bolt in a bearing connection?
The steel manual permits 0.40Fu for shear stress (LRFD) for other grades of threaded rod. Would you use a different value for PT rod?
The rods are not post-tensioned beyond snug tight and are being used for convenience (material on hand).
The steel manual permits 0.40Fu for shear stress (LRFD) for other grades of threaded rod. Would you use a different value for PT rod?
The rods are not post-tensioned beyond snug tight and are being used for convenience (material on hand).