INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

ASME B16.5 1974

ASME B16.5 1974

ASME B16.5 1974

(OP)
jte sent data from 1977 edition of B16.5 for A181-1 flanges.  Need allowable pressure at 150F and 200F.  thanks for the help.

JPG

RE: ASME B16.5 1974

ANSI 16.5 - 1977, Material Group 1.4 (A181-I)

Class 150: 235 psig @ 100 deg. F, 215 psig @ 200 deg. F.
Class 300: 620 psig @ 100 deg. F, 560 psig @ 200 deg. F.

For 150 deg. F. use linear interpolation.

Good Luck,

NozzleTwister
Houston, Texas

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources