machining nitralloy type 135
machining nitralloy type 135
(OP)
i have been trying to find an insert that will hold up while turning nitralloy 135. an insert grade for roughing and finish turning along with spindle speeds and feeds would be helpful. any info would be appreciated






RE: machining nitralloy type 135
RE: machining nitralloy type 135