INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Alternatives to ASTM A105 for MSS-SP83 pipe unions

Alternatives to ASTM A105 for MSS-SP83 pipe unions

Alternatives to ASTM A105 for MSS-SP83 pipe unions

(OP)
MSS-SP83 for pipe unions specify the use of ASTM A105 for carbon steel material.  We are finding A105 very hard to source.  MSS-SP83 states that "Unions may be made from materials of other wrought material by agreement between the manufacturer and the purchaser but shall not be marked SP-83".  What are acceptable alternatives that are readily available?

RE: Alternatives to ASTM A105 for MSS-SP83 pipe unions

What type union are you looking for?

RE: Alternatives to ASTM A105 for MSS-SP83 pipe unions

(OP)
Sorry - a threaded pipe union.

RE: Alternatives to ASTM A105 for MSS-SP83 pipe unions

rbrez,

You're obviously looking talking to the wrong suppliers. ASTM A105 forged carbon steel is the material for 3000# carbon steel unions per MSS SP-83-2001.

You might try contacting the following manufacturers, Bonney Forge or Kemper Valve and Fittings, they both have websites.

Good luck,

NozzleTwister
Houston, Texas

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources