Qualifications for to butt small bore pipe to plate
Qualifications for to butt small bore pipe to plate
(OP)
If a welder is certified for B-U2a joint in the 3G and 4G position is he also qualified to fillet weld small bore pipe to plate?
INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS Come Join Us!Are you an
Engineering professional? Join Eng-Tips Forums!
*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail. Posting GuidelinesJobs |
Qualifications for to butt small bore pipe to plate
|
Qualifications for to butt small bore pipe to plateQualifications for to butt small bore pipe to plate(OP)
If a welder is certified for B-U2a joint in the 3G and 4G position is he also qualified to fillet weld small bore pipe to plate?
Red Flag SubmittedThank you for helping keep Eng-Tips Forums free from inappropriate posts. Reply To This ThreadPosting in the Eng-Tips forums is a member-only feature.Click Here to join Eng-Tips and talk with other members! |
ResourcesWhat is rapid injection molding? For engineers working with tight product design timelines, rapid injection molding can be a critical tool for prototyping and testing functional models. Download Now
The world has changed considerably since the 1980s, when CAD first started displacing drafting tables. Download Now
Prototyping has always been a critical part of product development. Download Now
As the cloud is increasingly adopted for product development, questions remain as to just how cloud software tools compare to on-premise solutions. Download Now
|
RE: Qualifications for to butt small bore pipe to plate
RE: Qualifications for to butt small bore pipe to plate
RE: Qualifications for to butt small bore pipe to plate
Have a nice day
Gerald Austin
Iuka, Mississippi
http://www.weldinginspectionsvcs.com
RE: Qualifications for to butt small bore pipe to plate
In 2004 code, the table is 4.10