INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

FRP RC Beams
3

FRP RC Beams

FRP RC Beams

(OP)
Has anyone used FRP rods as reinforcement in concrete beams. I am trying to obtain some design info.


RE: FRP RC Beams

2
ACI Committe 440 has a design guide fo rexactly what you speak of called "Guide for the Design and Construction of Concrete Reinforced with FRP Bars" (ACI 440.1R-01).

Contact ACI to obtain a copy of it.

www.aci-int.org

RE: FRP RC Beams

ACI 440
Also, obtain design values from the FRP supplier.
Concrete design (for bending) with FRP is more conservative than with conventional reinforcing.  Not all bent shapes are available when using FRP.  Development lengths are different.  A FRP supplier that I have used in the past is Hughes Brothers, Inc.  They have a web site and are fairly helpful, even on the design side of things.

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources