Welding aluminized to stainless - possible?
Welding aluminized to stainless - possible?
(OP)
Is it possible to weld aluminized HR steel to 409 SS? My limited resources say not. What say y'all?
Griffy
Griffy
INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS Come Join Us!Are you an
Engineering professional? Join Eng-Tips Forums!
*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail. Posting GuidelinesJobs |
Welding aluminized to stainless - possible?
|
RE: Welding aluminized to stainless - possible?
RE: Welding aluminized to stainless - possible?
Under any normal welding conditions, expect a very weak weld because of oxide and intermetallic compound layers.