INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Looking for ink with good adhesion and wear on plastic?

Looking for ink with good adhesion and wear on plastic?

Looking for ink with good adhesion and wear on plastic?

(OP)
What type of ink should I use to highlight part descriptions engraved on plastics such as UHMW, Ertalyte and Delrin. The ink should have good resistance to cleaning agents and good adhesion properties. FDA approved would be a plus.

RE: Looking for ink with good adhesion and wear on plastic?

Have you tried talking to specialists in the area - eg Printers.  There are tight guidelines for the marking of containers for pharmaceuticals and therefore I suggest finding a suitable label / container manufacturer and asking them.

Have you spoken to the plastic suppliers, because if they are iso 9000 certified then they will probably have methods for marking their products.

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources