INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

How can avoid sticking epoxic thermoset in the plunger?

How can avoid sticking epoxic thermoset in the plunger?

How can avoid sticking epoxic thermoset in the plunger?

(OP)
I'm working on a compression molding process with ERC, and I want to avoid the sticking material in the plunger I aprecited  your help with any suggestion.




sincerly
Vic.

RE: How can avoid sticking epoxic thermoset in the plunger?

Currently one of our divisions is using compression molding on a thermoset laminate.  They seem to put a bit of wax on the thermoset so when it gets compressed, it wont stick.

Don't know if this is exactly what you were looking for; but, it might help.

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources