INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Materials and adhesives for space based antennas

Materials and adhesives for space based antennas

Materials and adhesives for space based antennas

(OP)
Generic question on space based adhesives, is there a standard type used in space applications for hardware that is exposed to the suns rays?

Being one step more specific, has anyone experience bonding Hexcel honeycomb to any Microwave transparent dielectric skin for use in space applications, and if so which skin and which adhesive was used.

I am using Hexcel HR-310 with a Rogers 6002 type Teflon based thin skin material but will likely change the Rogers material to a Mylar/polyimide Dupont Pyralux. An adhesive suggestion (room temp cure preferred) for this space application would be appreciated.

Thanks,
kch

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources