INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Best tester for PMI on material

Best tester for PMI on material

Best tester for PMI on material

(OP)
Hi.

We'd appreciate an advise on what tester is the best for
PMI on material and welding.
Our main application:
- SS : 304H
- CrMo: 1 1/4Cr 1/2 MO
Thanks in advance.

RE: Best tester for PMI on material

The common portable x-ray fluorescence units for PMI are;
Niton, Texas Nuclear and Inovex

They each have their advantages and disadvantages. These three will not determine carbon content. However, for general sorting of alloys and weld metal composition we use the Texas Nuclear, and a good magnet.

RE: Best tester for PMI on material

Spectro Analytical or Arc Met spectroscopic analyzers will give you specific carbon content of high and low carbon stainless steels.  The Niton, Texas Nuclear or Innovex will not.

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources