INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

6061-T6 Aluminum

6061-T6 Aluminum

6061-T6 Aluminum

(OP)
Can someone tell me what the 'T6' stands for in 6061-T6 aluminum? And is there a chart around somewhere defining the available 6061 suffixes?
Thanks,
Chris

RE: 6061-T6 Aluminum

The T6 is temper designation: Solution heat-treated, artificially aged. More info on these designations should be available on internet, try google.

RE: 6061-T6 Aluminum

The T6 refers to a specific heat treatment condition because this aluminum alloy can be age hardened. Here is a web site that I have used for various aluminium alloys with reference to suffix designations;

http://aluminium.matter.org.uk/aluselect/06_compos...

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources