INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

AMS 6504

AMS 6504

AMS 6504

(OP)
Hi all,
Does anybody know a link to show me the following standard?
AMS 6504

RE: AMS 6504

You will have to buy it or find a library that payed for it. Only MIL-STD's are free on the web.

RE: AMS 6504

(OP)
Does anybody know its composition?

RE: AMS 6504

Are you sure that this is AMS 6504? I did a search on Google and other search databases and didn't find any mention of such AMS standard. I searched MIL-HDBK-5J and ASSIST-QuickSearch too and didn't find anything so I assume it is not a spec for an aerospace metal. Can you give info what it dealing with (Materials, Metals, Testings, Coatings etc.)?

RE: AMS 6504

There is no standard SAE AMS6504.  Please confirm the designation that was given to you.

RE: AMS 6504

AMS5604  ???
Steel, Corrosion Resistant, Sheet, Strip, and Plate 16.5Cr 4.0Ni 4.0Cu 0.30Cb, Solution Heat Treated, Precipitation Hardenable

Abstract:  This specification covers a corrosion-resistant steel in the form of sheet, strip, and plate.

These products have been used typically for parts requiring corrosion resistance and high strength up to 600 degrees F (316 degrees C) and where such parts may require welding during fabrication, but usage is not limited to such applications.

Certain processing procedures and service conditions may cause these products to become subject to stress-corrosion cracking; ARP1110 recommends practices to minimize such conditions.

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources