INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Wet H2S

Wet H2S

(OP)
Hello Everybody,

How I can define if such service is a wet H2S service? Is it as a function of partial pressure of H2S at given temperature and pressure?

What is the definition of Wet H2S service (wet sour gas)?

RE: Wet H2S

H2S is a chemical formula for Hydrogen Sulfide. I am not quite sure about the wet H2s you have describe. But I guess your hydrogen sulfide is contaminated with water.

RE: Wet H2S

Most pipeline tarrifs limit H2S content to 0.25 grains per 100 SCF.  Furthermore, if the H2S content exceeds this value then the receiving pipeline has the right to shut in the source which is serious business.

You might also check the applicable NACE spec (10????) for a definition.  If the H2S content exceeds the value stated therein then you need to purchase all valves, meters, instrumentation, etc. with NACE trim.

Total sulfur is also limited but I do not remember the value now.

Water content is usually limited to 7 lbs/MMSCF in southern states and 4 in northern states.  The pipeline tarrif will also state no free water.  So if you have free water at your operating conditions then you have a wet gas.

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources