INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Stress-Strain Data

Stress-Strain Data

Stress-Strain Data

(OP)
What are the best public sources for stress-strain data on various rubber materials?

RE: Stress-Strain Data

We were looking for the same info all summer - we came to find out that due to the more "recent" nature of most elastomer developments and the widely varied ways casting and molding houses do their work - there are generally not too many curves out there.  We ended up building our own small test machine to develop curves and are still doing so in an onging manner.  SOME manufacturers can do testing and may supply you with curves for various materials.  One that I know of that has capabilities like this is:

http://www.glscorporation.com/

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources