Shear Modulus of Masonry
Shear Modulus of Masonry
(OP)
Does anyone know what the shear modulus of elasticity of masonry would be, or where i can find that information?
Thanks,
PAT2
Thanks,
PAT2
When was the last time you drove down the highway without seeing a commercial truck hauling goods?
Download nowINTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS Come Join Us!Are you an
Engineering professional? Join Eng-Tips Forums!
*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail. Posting GuidelinesJobs |
|
RE: Shear Modulus of Masonry
Check out ACI 530-02 section 1.8. Shear modulus can be taken as .4Em. Em = 700 f'm for clay masonry, and 900 f'm for concrete masonry.