INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

How to remove Loctite620
3

How to remove Loctite620

How to remove Loctite620

(OP)
Hi,
  Would like to know, other than heating, is there any chemical that can remove Loctite 620?

Regards.

RE: How to remove Loctite620

Locktite did make a remover.
Several other people also marketed a debonder. Look in Grainger's or McMaster-Carr's catalogue.  Another good place to check is some of the larger bearing houses.

RE: How to remove Loctite620

Many gun cleaners like for example Hoppes#9 will soften most Loctite compounds.

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources