INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Biaxial Bending of Concrete Column / Beam

Biaxial Bending of Concrete Column / Beam

Biaxial Bending of Concrete Column / Beam

(OP)
I have a concrete frame with biaxial bending in the beams and columns.  I'm wondering if anybody knows of any GOOD literature or examples on this topic.  I've been trying to go through an example by Edward Nawy but I've been getting lost in the process.  Basically, my moments are high relative to the compression in most cases but I can't find anything on biaxial bending of a beam with negligible axial load.  

I appreciate any help.

RE: Biaxial Bending of Concrete Column / Beam

"Reinforced Concrete" by Warner, Rangan and Hall (ISBN 0 582 71226 2) addresses biaxial bending in both beams and columns and has worked examples.  They reference the following paper in the chapter that includes a treatment of biaxial bending in beams:
   Warner, R.F.,
   'Biaxial Moment-Thrust-Curvature Relations',
   Journal of the Structural Division, ASCE,
   Vol. 98, No. ST5, 1972.

The Australian Standard, AS3600 "Concrete structures" addresses combined actions in reinforced concrete columns.  Some papers referenced in AS3600 are:
   Bresler, B.,
   ‘Design Criteria for Reinforced Concrete Columns Under Axial Load and Biaxial Bending’,
   ACI Journal,
   Vol. 57, No. 5, 1960, pp. 481–90.

   Chen, W.F. and Atsuta, T.,
   ‘Interaction Equations for Biaxially Loaded Sections’,
   Journal of the Structural Division, ASCE,
   Vol. 98, No. ST7, 1972, pp. 1035–52.

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources