Greetings;
Has anyone heard of any uses for carbon fullerenes in steel? A lot of hype over these structures when they were first discovered. Just wondering if any good R&D has been done lately on possible applications in steel. Gerald
Has anyone heard of any uses for carbon fullerenes in steel? A lot of hype over these structures when they were first discovered. Just wondering if any good R&D has been done lately on possible applications in steel. Gerald





RE: Fullerene applications in steel?
Carbon dissolves in molten iron, regardless of its original structure.
RE: Fullerene applications in steel?