RE: Coefficient friction for material combinations
They are listed in the CRC Handbook of Chemistry and Physics.
If you have enough load or motion that you expect wear, then you are not talking about simple friction any more and you need to find mixed couple wear data.
= = = = = = = = = = = = = = = = = = = =
Corrosion never sleeps, but it can be managed.
http://www.trenttube.com/Trent/tech_form.htm
RE: Coefficient friction for material combinations