INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

I - I diagram AISI 8680

I - I diagram AISI 8680

I - I diagram AISI 8680

(OP)
I would like to know who can send me the I-T diagram of the AISI 8680 steel and AISI 8620 steel. I will appreciate it a lot. My email adress is e9303251@pucp.edu.pe. Thanks. Pucp

RE: I - I diagram AISI 8680

Information on AISI and SAE alloys is available in volume 1 of the SAE handbook in specification SAE J1268 "Hardenability bands for carbon and alloy steels" available from any good library or SAE affiliate.

Good Luck

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources